Thick-Film Epoxy Anti-Corrosion Paint for Ship Bottoms - Iron Red by China Suppliers & Factory
Product Characteristics
Recommendations
Product Parameters
| Project | Data | ||||
| Density (Kg/L) | 1.45 | ||||
| Color | Iron Red | ||||
| Solid percentage by volume % | 72 ± 2 | ||||
| Reference dry film thickness (μm) | 125 | ||||
| Theoretical coating rate (㎡/L) | 5.8 | ||||
| Flash point | 30°C [86°F] | ||||
| Volatile matter (g/L) | 225 | ||||
| Gloss | Matte | ||||
| Drying time | 10℃ | 20℃ | 30℃ | ||
| Dry to touch | 180 mins | 120 mins | 90 mins | ||
| Actual drying | 24 hrs | 10 hrs | 8 hrs | ||
| Coating interval | 10℃ | 20℃ | 30℃ | ||
| Min | 8 hrs | 6 hrs | 4 hrs | ||
| Max | 15 Days | 8 Days | 5 Days | ||
| Potlife | 10℃ | 20℃ | 30℃ | ||
| 6 hrs | 4.5 hrs | 4 hrs | |||
| Mixing ratio | Base : Hardener (4:1 by volume) | ||||
| Storage period | 24 months at 25°C | ||||
Application
Airless spraying
Nozzle pressure: 14 MPa – 21 MPa
Nozzle hole diameter: 0.6 mm – 0.8 mm
If applying by brush or roller, additional coats will be required to achieve the specified dry film thickness. Spray data is for reference only and may be adjusted. Pressure is applicable to material temperatures of 20°C [68°F]. Brush and roller application is only suitable for line marking and small area touch-ups.
During construction and curing, the surface temperature of the substrate must be above 5°C [41°F].
To avoid condensation, the substrate temperature during construction should be at least 3°C [5°F] higher than the dew point, clean and dry.
Relative humidity: The relative humidity during construction and curing must be less than 85%.
Remove oil, grease and other contaminants with a suitable cleaning agent.
High-pressure water cleaning removes salt, detergents and other contaminants.
Surface blasted to Sa 2½ (ISO 8501-1) / SP 10 (SSPC).
Remove dust, sand and loose materials.
Surface blasted to PSa 2½ (ISO 8501-2) / SP 10 (SSPC).
High pressure water is sprayed onto Wa 2½ (ISO 8501-4).
Small areas can be cleaned by hand or electric tools instead of sandblasting.
The degree of flash rust is not higher than FR L (ISO 8501-4).
The surface of the substrate reaches Medium (G) (ISO 8503-2).