EP20901 Epoxy Vinyl Acrylate Coating
Product Features
In the amphiphilic resin system, the tie-coat typically employs modified epoxy resin or copolymers containing compatible groups, enabling one side to bond well with the epoxy primer and the other side to be compatible with the vinyl topcoat.
With good wettability and permeability, it can effectively wet the surface of epoxy coatings, forming strong physical/chemical bonds.
It has strong adaptability in construction, can be sprayed and brushed, and has a moderate drying time, making it suitable for shipyard environments
Resistant to salt spray and seawater, meeting the requirements for ships to be exposed to marine corrosive environments for extended periods.
Recommended Use
Used for the combined application of anti-corrosion primer and anti-fouling paint in new shipbuilding and old ship maintenance.
Product Parameters
| Project | Data | |||
| Density (Kg/L) | 1.4 | |||
| Color | grey | |||
| Solid percentage by volume % | 57 ± 2 | |||
| Reference dry film thickness (μm) | 100 | |||
| Theoretical coating rate (㎡/L) | 5.7 | |||
| Flash point | 38°С [100°F] | |||
| Volatile matter (g/L) | 396 | |||
| Gloss | No light | |||
| Drying time | 10℃ | 20℃ | 30℃ | |
| Dry to touch | 3hrs | 1.5hrs | 1hrs | |
| Actual drying | 24hrs | 10hrs | 8hrs | |
| Coating interval | 10℃ | 20℃ | 30℃ | |
| min | 24hrs | 10hrs | 8hrs | |
| Potlife | 10℃ | 20℃ | 30℃ | |
| 10hrs | 8hrs | 6hrs | ||
| Mixing ratio | Main agent: curing agent (4:1 volume ratio) | |||
| Storage period | 24 months 25°C | |||
Application
Construction method:
Airless spraying
Nozzle pressure: 14 MPa -21 MPa
Nozzle hole diameter: 0.6mm-0.8mm
Surface treatment and construction conditions:
To avoid condensation, please apply on a clean and dry surface with a temperature at least 3 ° C [5 ° F] above the dew point
The surface of the primer should be dry and free of any contaminants (oil, grease, salt, water, dust, etc.), and should be recoated within the specified recoating interval
The relative humidity during construction and curing process must be less than 85%
Disclaimer
The information provided in this manual is the most comprehensive and correct information we have at present. Since the conditions of product use are beyond our control, the information here does not contain any guarantee, that is, we are only responsible to the buyer for the product selection. Due to the continuous development of our company's products and production processes, all information here is subject to our confirmation.